Polymer Property : Shear Modulus = 2.74411 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.50857 - 2.74411 GPa

@Temperature -100 - 0.000 °C
218.803 - 398.006 ksi

@Temperature -148 - 32.0 °F
Average value: 2.10 GPa Grade Count:3
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..