Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.141 - 2.432 GPa @Temperature -50.0 - 250 °C |
20.5 - 352.7 ksi @Temperature -58.0 - 482 °F |
Average value: 1.13 GPa Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |