Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 159 GPa | 23100 ksi | Calculated |
CeramTec V 679 Alumina, 99.7% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Shear Modulus | 159 GPa | 23100 ksi | Calculated |
CeramTec AT 79 Alumina, 99.6% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |