Shear Modulus 26.0 GPa
3770 ksi
calculated
Schott KZFS12 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 26.0 GPa
3770 ksi
calculated
Schott SF10 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 26.0 GPa
3770 ksi
calculated
Schott N-KZFS2 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 26.0 GPa
3770 ksi
Corning Gorilla® Glass 4 Touch Screen Glass
Gorilla® Glass 4 is just as thin and light as previous versions of Gorilla® Glass, but has been formulated to deliver dramatically improved damage resistance allowing improved in-field performance..