Polymer Property : Shear Modulus = 28.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 28.0 GPa
4060 ksi
calculated
Schott K7 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 28.0 GPa
4060 ksi
calculated
Schott N-FK51A Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Shear Modulus 28.0 GPa
4060 ksi
Corning Vycor® 7913 UV-Transmitting Glass
Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to high temperatures.Excellent thermal shock resistanceTypical Applications:Halogen l..
Shear Modulus 28.0 GPa
4060 ksi
Corning Vycor® 7950 Red Glass
Used to reduce the light of quartz lamps (blocks most visible white light while transmitting IR). One specific use is blocking glare from heating units.Special Features:Superior optical qualityTigh..