Polymer Property : Shear Modulus = 3.25 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 3.25 GPa
471 ksi
Calculated
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)  (discontinued **)
Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..