Mechanical Properties Metric English Comments
Shear Modulus 2.10 GPa
305 ksi
calculated
BASF Capron® HPN 9315G Impact Modified, 15% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9315G is a 15% glass reinforced, impact modified polyamide 6 injection molding grade resin in the High Productivity Nylon Series developed for applications requiring superior dry-as-molde..