Polymer Property : Shear Modulus = 35.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 2.96475 - 35.0 GPa

@Temperature 80.0 - 175 °C
430.007 - 5080 ksi

@Temperature 176 - 347 °F
Average value: 13.7 GPa Grade Count:2
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..