Mechanical Properties Metric English Comments
Shear Modulus 4.15 - 4.36 GPa
602 - 632 ksi
Calculated
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry  (discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..