Mechanical Properties Metric English Comments
Shear Modulus 4.39 GPa
637 ksi
Calculated
Plenco 1501 Polyester, Briquette, Transfer Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..