Shear Modulus 4.756 GPa
689.8 ksi
ASTM C273
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK
LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.