Mechanical Properties Metric English Comments
Shear Modulus 43.0 GPa
6240 ksi
calculated
Schott N-LASF40 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 43.0 GPa
6240 ksi
calculated
Schott N-LAF33 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 -0.05Pd Titanium Alloy
Cold Workable Medium Strength Alloy. Palladium is added to this grade to enhance its corrosion behavior. Property data below is typical of TIMETAL® 3-2.5 Titanium Alloy.Data provided by TIMET.
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Aged
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to aged material; other specific condition entries are also available in MatWeb.Features: Cold formable and we..
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed
Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.Features..
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties
Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v..
Shear Modulus 43.0 GPa
6240 ksi
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy;
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w..
Shear Modulus 43.0 GPa
6240 ksi
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
Shear Modulus 43.0 GPa
6240 ksi
calculated
Schott N-LAK14 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 43.0 GPa
6240 ksi
calculated
Schott N-LAK9 Glass
Information Provided by SCHOTT North America, Inc.