Polymer Property : Shear Modulus = 458 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 3.16 GPa
458 ksi
Calculated
Plenco 4301 Phenolic, Granular, Injection Molded
PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava..