Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.342 - 5.18 GPa | 49.6 - 751 ksi | Average value: 2.60 GPa Grade Count:7 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |