Polymer Property : Shear Modulus = 5.00 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.0345 GPa
5.00 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP - 1/4 - 3.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Modulus 0.0345 GPa
5.00 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Modulus 0.0345 GPa
5.00 ksi
Plate Shear, W Direction, typ, preliminary value obtained from limited testing
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..