Mechanical Properties Metric English Comments
Shear Modulus 3.42 - 5.11 GPa
496 - 741 ksi
Calculated
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..