Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.19 GPa | 753 ksi | Calculated |
Plenco 08122 Polyester BMC, Compression Molded PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Shear Modulus | 5.19 GPa | 753 ksi | Calculated |
Premix Premi-Glas® 1281-32 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1281-32 VE SMC is a high strength glass reinforced vinyl ester sheet molding compound formulated for under-the-hood automotive applications. Key features and benefits: Desi.. |