Mechanical Properties Metric English Comments
Shear Modulus 5.43 - 5.75 GPa
788 - 834 ksi
Calculated
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..