Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.00 - 5.82 GPa | 435 - 844 ksi | Average value: 3.73 GPa Grade Count:14 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |