Polymer Property : Shear Modulus = 5080 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-BAF10 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-BAF52 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-SF10 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-SF14 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-LAK7 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-SF2 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-SF5 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-SF8 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-SK16 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa
5080 ksi
calculated
Schott N-BAF4 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 35.0 GPa

@Temperature 80.0 °C
5080 ksi

@Temperature 176 °F
In-Plane Shear, Wet; AiTM 1.0002
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System
HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process...