Polymer Property : Shear Modulus = 547 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 3.77 GPa
547 ksi
Calculated
Plenco 4527 Phenolic, Granular, Injection Molded
PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under..