Polymer Property : Shear Modulus = 59.3 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus >= 0.409 GPa

@Temperature -50.0 - 200 °C
>= 59.3 ksi

@Temperature -58.0 - 392 °F
Average value: 1.41 GPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..