Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0462 GPa | 6.70 ksi | Plate Shear, L Direction |
Hexcel® HexWeb® HRH-36/OX - 3/16 - 3.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |