Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0469 GPa | 6.80 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/8-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |