Mechanical Properties Metric English Comments
Shear Modulus 4.43 GPa
643 ksi
Calculated
Plenco 1581 Polyester, Pellet, Injection Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..
Shear Modulus 4.43 GPa
643 ksi
Calculated
Plenco 1586 Polyester, Pellet, Injection Molded
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti..