Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 4.47 GPa | 648 ksi | Calculated |
Plenco 7552 Phenolic, Nodular, Injection Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |