Polymer Property : Shear Modulus = 653 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 4.50 GPa
653 ksi
ASTM D4065
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC