Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 77.2 GPa | 11200 ksi | |
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
Shear Modulus | 77.2 GPa | 11200 ksi | |
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Shear Modulus | 77.2 GPa | 11200 ksi | H900 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Shear Modulus | 77.2 GPa | 11200 ksi | H900 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Shear Modulus | 77.2 GPa | 11200 ksi | H900 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Shear Modulus | 77.2 GPa | 11200 ksi | |
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |