Mechanical Properties Metric English Comments
Shear Modulus 5.85 GPa
848 ksi
Calculated
Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..