Polymer Property : Shear Modulus = 9000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 62.1 GPa
9000 ksi
Crucible Steel 422 Stainless Steel
Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is..
Shear Modulus 62.1 GPa
9000 ksi
Short Beam; 0° stress angle; span/depth 5:1; ASTM D2344-76; span/depth 5:1
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..