Shear Modulus 91.0 GPa
13200 ksi
Calculated
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..