Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 65.5 GPa | 9500 ksi | |
Meehanite AQ Flake Graphite Cast Iron Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate.. |
|||
Shear Modulus | 65.5 GPa | 9500 ksi | |
Meehanite GM-60 Flake Graphite Cast Iron Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a.. |
|||
Shear Modulus | 65.5 GPa | 9500 ksi | Short Beam; 0° stress angle; span/depth 5:1; ASTM D2344-76; span/depth 5:1 |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Shear Modulus | 65.5 GPa | 9500 ksi | |
Carlson C 400 Nickel-Copper Alloy General DescriptionCarlson Alloy C 400 is a nickel-copper alloy which provides an excellent combination of high strength, ductility, good weldability, and resistance to corrosion over a wide range o.. |