Polymer Property : Dart Drop = 3.60 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 3.60 g/micron

@Temperature -30.0 °C
91.4 g/mil

@Temperature -22.0 °F
ASTM 1709A
Eastman Tritan FX100 Copolyester
Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..