Mechanical Properties Metric English Comments
Torsional Stiffness 310 MPa

@Temperature 13.0 °C
45000 psi

@Temperature 55.4 °F
Plasticizer conc. in vinyl film 33 phr; ASTM D1043
BASF Palamoll® 656 Polymeric Plasticizer
Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro..
Torsional Stiffness 310 MPa

@Temperature -18.0 °C
45000 psi

@Temperature -0.400 °F
Plasticizer conc. in vinyl film 67 phr; ASTM D1043
BASF Palamoll® 656 Polymeric Plasticizer
Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro..
Torsional Stiffness 310 MPa

@Temperature -15.0 °C
45000 psi

@Temperature 5.00 °F
Plasticizer conc. in vinyl film 40 phr; ASTM D1043
BASF Palatinol® 11P-E (DUP) Linear Phthalate
Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing ..
Torsional Stiffness 310 MPa

@Temperature -30.0 °C
45000 psi

@Temperature -22.0 °F
Plasticizer conc. in vinyl film 50 phr; ASTM D1043
BASF Palatinol® 11P-E (DUP) Linear Phthalate
Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing ..
Torsional Stiffness 310 MPa

@Temperature -45.0 °C
45000 psi

@Temperature -49.0 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D1043
BASF Palatinol® 11P-E (DUP) Linear Phthalate
Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing ..
Torsional Stiffness 310 MPa

@Temperature -9.00 °C
45000 psi

@Temperature 15.8 °F
Plasticizer conc. in vinyl film 40 phr; ASTM D1043
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..
Torsional Stiffness 310 MPa

@Temperature -22.0 °C
45000 psi

@Temperature -7.60 °F
Plasticizer conc. in vinyl film 50 phr; ASTM D1043
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..
Torsional Stiffness 310 MPa

@Temperature -38.0 °C
45000 psi

@Temperature -36.4 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D1043
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..