Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 100 °C |
200 g/in @Pressure 0.500 psi, Temperature 212 °F |
0.5 sec, LPS; ExxonMobl Method |
ExxonMobil Bicor™ 21MB621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an.. |
|||
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 100 °C |
200 g/in @Pressure 0.500 psi, Temperature 212 °F |
LSP, 0.5 sec; ExxonMobil Method |
ExxonMobil Bicor™ 26MB600 OPP Film Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia.. |
|||
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 100 °C |
200 g/in @Pressure 0.500 psi, Temperature 212 °F |
LPS, 0.5 sec; ExxonMobil Method |
ExxonMobil Bicor™ 32MB600 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As.. |
|||
Seal Strength | 200 g/25 mm @Pressure 0.00345 MPa, Temperature 100 °C |
200 g/in @Pressure 0.500 psi, Temperature 212 °F |
LPS, 0.5 sec; ExxonMobl Method |
ExxonMobil Bicor™ 52MBR666 OPP Film Product Description: Bicor 52MBR666 is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high mo.. |