Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 560 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
560 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Bruger, 0.2 sec, Acrylic; ExxonMobl Method |
ExxonMobil Bicor™ 21MB777 OPP Film Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m.. |