Mechanical Properties Metric English Comments
Izod Impact Resistance 0.500 J/cm²

@Temperature -40.0 °C
2.38 ft-lb/in²

@Temperature -40.0 °F
cond; ISO 180/1A
DSM Stanyl® TE351 PA46 FR(17)
Flame Retardant, Heat Stabilized
Izod Impact Resistance 0.500 J/cm²

@Temperature -40.0 °C
2.38 ft-lb/in²

@Temperature -40.0 °F
dry; ISO 180/1A
DSM Stanyl® TE351 PA46 FR(17)
Flame Retardant, Heat Stabilized
Izod Impact Resistance 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 180/1A
DSM Stanyl® TW241B3 PA46-CF15
15% Carbon Reinforced, Heat Stabilized, Lubricated