Mechanical Properties Metric English Comments
Izod Impact Resistance 1.10 J/cm²

@Temperature -40.0 °C
5.24 ft-lb/in²

@Temperature -40.0 °F
cond; ISO 180/1A
DSM Stanyl® TS200F6 PA46-GF30
30% Glass Reinforced
Izod Impact Resistance 1.10 J/cm²

@Temperature -40.0 °C
5.24 ft-lb/in²

@Temperature -40.0 °F
dry; ISO 180/1A
DSM Stanyl® TS200F6 PA46-GF30
30% Glass Reinforced