Polymer Property : Film Tensile Strength at Yield, TD = 12.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 12.5 MPa
1810 psi
ASTM D882
Iran Petrochemical (PCC) LL22501 Linear Low Density Polyethylene
22501 is a high stiffness LLDPE blown film grade designed for applications requiring good optical properties even at low extrusion temperature. This resin combines ease of processing with low gels a..
Film Tensile Strength at Yield, TD 12.5 MPa
1810 psi
ASTM D882
Dow ELITE™ 5100G Enhanced Polyethylene Resin
™ 5100G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers excellent impact strength, good tensile and puncture properties for thick and thin gauge industrial and consume..