Film Tensile Strength at Yield, TD 19.3 MPa
2800 psi
ASTM D882, A
Total MDPE HL 323 Medium Density Polyethylene, Film Resin
Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st..
Film Tensile Strength at Yield, TD 19.3 MPa
2800 psi
ASTM D882
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin
Product Description: Enable 35-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Yield, TD 19.3 MPa
2800 psi
ASTM D882
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 35-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..