Polymer Property : Film Tensile Strength at Yield, TD = 19.73 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 19.73 MPa
2862 psi
ASTM D882
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th..