Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 24.1 - 41.4 MPa | 3500 - 6000 psi | ASTM D882 |
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film
(discontinued **) Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc.. |
|||
Film Tensile Strength at Yield, TD | 24.1 MPa | 3500 psi | ASTM D 882 A |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |