Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 26.9 MPa
3900 psi
ASTM D882
LyondellBasell Alathon® L5845 High Density Polyethylene
ApplicationsALATHON L 5845 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include paper replacement, coextrusions and laminations.Reg..
Film Tensile Strength at Yield, TD 26.9 MPa
3900 psi
ASTM D882
LyondellBasell Alathon® L4907 High Density Polyethylene
ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro..