Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 19.0 MPa | 2760 psi | ISO 1184 |
SIDPEC EGYPTENE® HD 3802 FA HDPE Film Applications:General purpose thin film, trash bags, merchant bagsBlending partnerFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 10D neck height.Information provi.. |
|||
Film Tensile Strength at Yield, TD | 19.0 MPa | 2760 psi | ISO 527-3 |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |
|||
Film Tensile Strength at Yield, TD | 19.0 MPa | 2760 psi | ASTM-D882 |
Braskem RP 344 RACO Random Polypropylene Copolymer RP 344 is a medium melt flow rate random copolymer. It is suitable for blown and cast film extrusion and features good processability, excellent optical properties, and outstanding sealability. Its .. |