Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 28.3 MPa
4100 psi
ASTM D882
Honeywell Stretch-Vac® 2000 Heat-Stabilized Blown Film  (discontinued **)
Description: Stretch-Vac® 2000 is a pink tinted, high elongation, heat-stabilized blown film produced from modified polyamide resin. It is available in widths up to 80 inches as layflat tubing and..
Film Tensile Strength at Yield, TD 28.3 MPa
4100 psi
ASTM D882
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Grade
PETROTHENE LP510300 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. LP510300 is recommended ..
Film Tensile Strength at Yield, TD 28.3 MPa
4100 psi
Dow HDPE 05862N High Density Polyethylene
Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
Film Tensile Strength at Yield, TD 28.3 MPa
4100 psi
ASTM D882
Honeywell Stretch-Vac® Elastomax 1000 Heat-Stabilized Blown Film  (discontinued **)
Description: Capran® Elastomax 1000 is a pink tinted, heat-stabilized blown film produced from modified nylon resin. It is available in widths up to 80 inches as layflat tubing and 120 inches as s..