Polymer Property : Film Tensile Strength at Yield, TD = 3480 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 22.0 - 24.0 MPa
3190 - 3480 psi
Average value: 23.0 MPa Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim..