Film Tensile Strength at Yield, TD 23.0 - 37.5 MPa
3340 - 5440 psi
Average value: 31.1 MPa Grade Count:5
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..