Polymer Property : Film Tensile Strength at Yield, TD = 4410 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 30.4 MPa
4410 psi
25.4 microns; ASTM D882
Dow 118.01 Developmental Performance Polypropylene Polymer
D118.01 Developmental Performance Polymer is a propylene-based resin intended for use in film, sheet extrusion and injection molding applications. Film and sheet produced from this resin offer impr..