Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | >= 32.0 MPa | >= 4640 psi | ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Film Tensile Strength at Yield, TD | >= 32.0 MPa | >= 4640 psi | ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |