Polymer Property : Film Tensile Strength at Yield, TD = 5.45 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 5.45 MPa
790 psi
ASTM D882
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g..